Browse Prior Art Database

HIGH MOLECULAR WEIGHT TONER WITH LOW FUSING TEMPERATURE USING A SOLID PLASTICIZER

IP.com Disclosure Number: IPCOM000023080D
Original Publication Date: 1976-Aug-31
Included in the Prior Art Database: 2004-Mar-27
Document File: 2 page(s) / 162K

Publishing Venue

Xerox Disclosure Journal

Abstract

It is disclosed that solid plasticizers may be used in toner materials, Such solid plasticizers act as fillers below their melting points thereby increasing modulus of the polymer material as long as the plasticizers are below their melting point, The solid plasticizers, when

This text was extracted from a PDF file.
At least one non-text object (such as an image or picture) has been suppressed.
This is the abbreviated version, containing approximately 100% of the total text.

Page 1 of 2

~XD~SCLOSUREJOURNAL

HIGH MOLECULAR WEIGHT TONER Proposed Classification
WITH LOW FUSING TEMPERATURE U~S, Cl~ 252/62,1
USING A SOLID PLASTICIZER Int, Cl, G03g 9/00

Thomas C~ Warren

It is disclosed that solid plasticizers may be used in
toner materials, Such solid plasticizers act as fillers
below their melting points thereby increasing modulus of

the polymer material as long as the plasticizers are
below their melting point, The solid plasticizers, when

heated above their melting point, act as plasticizers
and lower the viscosity~ Many solid plasticizers are
known with molecular weights of above 300 and melting

points suitable for toner applications, i,e,, o~- and

p~toluene sulfonamide, triethylene glycol dibenzoate,
triphenyl phosphate, diphenyl phthalate, glyceryl tri~
benzoate, N~ethyl-p-toluene sulfonamide, dicyclohexyl
phtha late,

Volume 1 Number 8 August 1976 41

[This page contains 1 picture or other non-text object]

Page 2 of 2

42 XEROX DISCLOSURE JOURNAL

Volume 1 Number 8 August 1976

[This page contains 1 picture or other non-text object]