Rework Procedure for 3M™ Plastic Bonding Adhesive 2665 or Equivalent Adhesive when used for Display Applications in Smart Phones

IP.com Disclosure Number: IPCOM000211153D
Publication Date: 2011-Sep-22
Document File: 3 page(s) / 586K

Publishing Venue

The IP.com Prior Art Database

Abstract

This paper describes a rework procedure for a touch display. The procedure involves delaminating the touch display from its housing. A thermal process is used to weaken the bond strength of the adhesive, which holds the display to the housing. The weakened adhesive allows the touch display to be removed from the housing, thus facilitating the rework process.